About this deal
Liu JF, Zhang Y, Hadjipanayis GC. High-temperature magnetic properties and microstructural analysis of Sm(Co, Fe, Cu, Zr) z permanent magnets. J Magn Magn Mater. 1999;202(1):69.
Zhang ZX, Song XY, Xu WW. Phase evolution and its effects on the magnetic performance of nanocrystalline SmCo 7 alloy. Acta Mater. 2011;59(4):1808. Liu S, Potts G, Doyle G, Yang J, Kuhl GE, Chen C, Walmer MS. Effect of z value on high temperature performance of Sm(Co, Fe, Cu, Zr) z with z = 7.14–8.10. IEEE Trans Magn. 2000;36(5):3297. Liu D, Liu XM, Liu GQ, Song XY. Phase stability and magnetic performance of nanocrystalline Sm–Co supersaturated solid solution. Sci China Technol Sci. 2018;61(1):129. Zhang TL, Liu HY, Liu JH, Jiang CB. 2:17-type SmCo quasi-single-crystal high temperature magnets. Appl Phys Lett. 2015;106(16):162403.Goll D, Kronmüller H, Stadelmaier HH. Micromagnetism and the microstructure of high-temperature permanent magnets. J Appl Phys. 2004;96(11):6534. Liu S, Yang J, Doyle G, Potts G, Kuhl GE. Abnormal temperature dependence of intrinsic coercivity in sintered Sm–Co-based permanent magnets. J Appl Phys. 2000;87(9):6728. Peng L, Yang QH, Zhang HW, Xu GL, Zhang M, Wang JD. Rare earth permanent magnets Sm 2(Co, Fe, Cu, Zr) 17 for high temperature applications. J Rare Earth. 2008;26(3):378. Chen CH, Walmer MS, Walmer MH, Liu S, Kuhl E, Simon G. Sm 2(Co, Fe, Cu, Zr) 17 magnets for use at temperature ≥ 400 °C. J Appl Phys. 1998;83(11):6706.
Guo ZH, Pan W, Li W. Sm(Co, Fe, Cu, Zr) z sintered magnets with a maximum operating temperature of 500 °C. J Magn Magn Mater. 2006;303(2):e396.
Huang G, Song XY, Liu D, Wang DX, Wang HB, Liu XM. Effects of Hf on phase structure and magnetic performance of nanocrystalline SmCo 7-type alloy. J Mater Sci. 2016;51(7):3390.
Walmer MS, Chen CH, Walmer MH. A new class of Sm-TM magnets for operating temperatures up to 550 °C. IEEE Trans Magn. 2000;36(5):3376. Yu NJ, Zhu MG, Fang YK, Song LW, Sun W, Song KK, Li W. The microstructure and magnetic characteristics of Sm(Co balFe 0.1Cu 0.09Zr 0.03) 7.24 high temperature permanent magnets. Scr Mater. 2017;132:44.Liu JF, Zhang Y, Dimitrov D, Hadjipanayis GC. Microstructure and high temperature magnetic properties of Sm(Co, Cu, Fe, Zr) z ( z = 6.7–9.1) permanent magnets. J Appl Phys. 1999;85(5):2800. Wang GJ, Jiang CB. The coercivity and domain structure of Sm(Co balFe 0.1Cu xZr 0.033) 6.9 ( x = 0.07, 0.10, 0.13) high temperature permanent magnets. J Appl Phys. 2012;112(3):033909.